Posted 2023-08-19 6:31 PM (#631435 - in reply to #631434) Subject: RE: Pot metal
Expert 5K+
Posts: 9924
Location: Lower Mainland BC
.
Here is one example of fixing pitting using "Muggy Weld" to fix pot metal pitting before plating, done by Gary S:
GaryS - 2018-09-04 11:37 AM
The "weld" part of the name is misleading. I used quite a lot of Muggy Weld filling pitted chrome and even replacing lead fill in body parts, but it doesn't do the job of welding anything.
Here is a wiper bezel for my '56 Plymouth that I filled and replated. Lots of work, but I'm satisfied.